Marginal and internal adaptation of stratified compomer-composite Class II restorations

DIETSCHI, Didier, et al.

Abstract

Different approaches have been proposed to improve the adaptation of Class II restorations, including applying low-elasticity modulus base liners. This in vitro fatigue test (or study) evaluated the influence of the compomer base-lining configuration on restoration adaptation.

Direct Class II MOD box-shaped composite restorations with or without base and lining (n=3x8) were placed on intact human third molars with proximal margins 1 mm above or under the CEJ. The compomer (Dyract) was applied as a 1 mm-thick lining or as a base, closing proximo-gingival margins. Marginal adaptation was assessed before and after each phase of mechanical loading (250,000 cycles at 50N, 250,000 cycles at 75N and 500,000 cycles at 100N); internal adaptation was evaluated after test completion. Gold-sputtered resin replicas were observed in the SEM and restoration quality evaluated in percentages of continuity (C) at the margins and within the internal interface after sample section. Mechanical loading did not influence adaptation to enamel, while it adversely affected restoration adaptation to dentin for the full composite and compomer-base [...]

DIETSCHI, Didier, et al . Marginal and internal adaptation of stratified compomer-composite Class II restorations. Operative Dentistry , 2002, vol. 27, no. 5, p. 500-9

PMID : 12216570

Available at:

http://archive-ouverte.unige.ch/unige:85026

Disclaimer: layout of this document may differ from the published version.

1 / 1

(2)
(3)
(4)
(5)
(6)
(7)
(8)
(9)
(10)
(11)

Références

Documents relatifs

To visualise the ultrastructure of the interface of SCA compomer adhesive and of Optibond composite adhesive in enamel and dentin, and to relate the findings to the marginal

After 500,000 and 1,000,000 loading cycles, the use of Prime & Bond, together with an immediate composite insertion (PB-IP), resulted in a marginal adaptation on

This in vitro study generated data on the quality of marginal adaptation, fracture resistance and retention of several indirect adhesive composite configurations on

Mean values of opened internal interface with dentin varied from 11.06% (Tetric Flow) to 28.15% (Prodigy). The present results regarding dentin adaptation confirmed that the

The marginal adaptation of the pit and fissure sealant restorations was evaluated by using a computer-assisted quantitative margin analysis in a scanning electron microscope (SEM)

lower results (Gr. Previous studies have shown that when preparing enamel by laser with an energy of 4 J, enamel temperature increased dramatically, inducing a

Two dentin types, i.e., sound and demineralized by formic-acid, were biomodified with 1% riboflavin and calcium phosphate (CaP) prior to the application of a universal

Six MOD inlay preparations of standardized design with one cervical margin in dentine and the other in enamel were prepared for each inlay type: CAD/CAM fabricated MGC-glass