International Conference on Advances in Mechanical Engineering

Volume 17, Issue 17, 2017, Pages 1-6

Estimated life time in an HDPE pipe with a semi-elliptical defect under internal pressure

L. Alimi, K. Chaoui, M. HASSANI, A. Azzi

Abstract: High density polyethylene has been widely used in marine and gas transportation, storm sewers, culverts and city drainage system. Compared with other conventional pipes, it has its own advantages, such as, chemical and corrosion resistance, toughness, flexibility, easy splicing and consequent easy handling and installation. In this paper, and in order to predict the remaining lifetime of a pipe having a defect and subjected to internal pressure, it is necessary to estimate KI stress intensity factor during the propagation of the crack. The finite element method is used to assess the values of the stress intensity factor of an axially oriented semi-elliptical crack located at the inner surface of an HDPE pipe. The crack configuration is described by the relative wall thickness (t/R), the relative crack depth (a/t) and the crack aspect ratio (a/c). The lifetimes presented are discussed according to the size of the crack and the stress intensity factor in each case.

Keywords : HDPE pipe, Crack, rupture, Finite Element Method FEM, stress intensity factor, Lifetime

Centre de Recherche en Technologies Industrielles - CRTI - www.crti.dz

Powered by TCPDF (www.tcpdf.org)

Références

Documents relatifs

When the Reynolds number is raised to 3500, neighboring secondary filaments locally interact with one another, flatten into vortex sheets, and split into smaller tertiary filaments,

KEY WORDS : dynamic fracture mechanics; numerical stability; energy balance; extended finite element method; dynamic stress intensity

2 groups: (1) The Rate Process Method or RPM, (2) The Bi-Directional Shift Approach, and (3) Methods of the Fracture Mechanics. In the latter category, there are several

decreased systematically for all toughness cases supporting the idea that reliability and fracture toughness designate similar properties for service life or material resistance

Lifetime man- agement of underground pipelines is mandatory for safety and the use of HDPE tubes subjected to internal pressure, external loading and environmental

Morphological properties such as crystallinity, crystalline lamellae thickness and the oxidation induction time (OIT) are studied using differential scanning calorimetry in order

This type of results allowed establishing the linear relationship between the elastic modulus and theyield stress and is intended to contribute to a better understanding of

Abstract : In this study, external and internal surfaces of a high density polyethylene (HDPE-100) pipe are characterized in terms of roughness and hardness in order to